Multiferroic solid solutions of Ba1−xLaxTi1−x/4O3 and iron (BLFT) were synthesized using the conventional mixed oxide method. The dependence of the piezoelectric coefficients on Fe content in BLFT ceramics was determined… Click to show full abstract
Multiferroic solid solutions of Ba1−xLaxTi1−x/4O3 and iron (BLFT) were synthesized using the conventional mixed oxide method. The dependence of the piezoelectric coefficients on Fe content in BLFT ceramics was determined by the quasi-static and resonance method. The results indicate that 0.3 mol% addition of Fe3+ ions to the ceramic structure increased the value of the piezoelectric parameter d33 to the maximum of 159 pC/N. This puts BLFT ceramics among other good-quality and lead-free piezoelectric ceramics. A major enhancement of dielectric properties related to the manipulation of Fe content in the barium lanthanum titanate (BLT) ceramics system is reported as well.
               