Abstract: Abstract The morphology of Zn deposit can be controlled by pulse deposition. Using defined pulse parameters (20 millisecond-on and 80 millisecond-off), the deposition current density was examined in 50–200 mA cm−2, in the electrolyte 9 M KOH + 5wt% ZnO,…