Investigation of {001} Texture Reservation and Grain Boundary Character Distribution of Fe–6.9 wt%Si Magnetic Material by Warm–Cold Rolling

Photo from wikipedia

In this work, the texture evolution, grain boundary character distribution, and magnetic properties of nonoriented Fe–6.9 wt%Si electrical steel are studied. It is found that Fe–6.9 wt%Si steel obtains the higher magnetic… Click to show full abstract

In this work, the texture evolution, grain boundary character distribution, and magnetic properties of nonoriented Fe–6.9 wt%Si electrical steel are studied. It is found that Fe–6.9 wt%Si steel obtains the higher magnetic inductions based on the heredity of {001} orientation texture during warm rolling, whereas the change in γ‐fiber recrystallization texture is attributed to a significant increase in the frequency of coincidence site lattice grain boundaries after annealing. Meanwhile, the increased recrystallization nuclei in the shear bands lead to the improvement of recrystallization nucleation rate and the decline of grain size because of the accumulation of internal stored energy. Finally, the values of magnetic inductions (B8, B50) and iron losses (P10/50, P10/400) decrease with increasing warm rolling temperatures.

Keywords: character distribution; texture; distribution magnetic; boundary character; grain boundary; grain

Journal Title: steel research international
Year Published: 2019

Link to full text (if available)


Share on Social Media:                               Sign Up to like & get
recommendations!

Related content

More Information              News              Social Media              Video              Recommended



                Click one of the above tabs to view related content.