The possibility is studied of preparing polymetal specimens of Ti and Ti–6Al–4V by direct laser deposition. The microstructure of deposited specimen zones given heat treatment shows a transition zone from… Click to show full abstract
The possibility is studied of preparing polymetal specimens of Ti and Ti–6Al–4V by direct laser deposition. The microstructure of deposited specimen zones given heat treatment shows a transition zone from (α+β) phase from the side of Ti–6Al–4V alloy to α-phase from the Ti side. No cracks are observed within the structure. With a change-over from Ti–6Al–4V to Ti microhardness varies from 380 to 200 HV.
               