High Purity Nickel Recovery from an Industrial Sidestream Using Concentration and Liquid–Liquid Extraction Techniques

Photo by justin_ziadeh from unsplash

This article outlines an alternative flowsheet for the purification of a multi-metal industrial sidestream (16.3 g/l Ni, 0.7 g/l Co, 0.6 g/l Ca and 1.6 g/l Mg) to allow high-purity nickel recovery. The methodology comprises… Click to show full abstract

This article outlines an alternative flowsheet for the purification of a multi-metal industrial sidestream (16.3 g/l Ni, 0.7 g/l Co, 0.6 g/l Ca and 1.6 g/l Mg) to allow high-purity nickel recovery. The methodology comprises an initial evaporation step to achieve Ca removal followed by impurity (Ca, Mg) and valuable (Co, Ni) element separation via two-step solvent extraction with organophosphorus extractants. Results indicate that > 80% of Ca is selectively removed as CaSO 4 ·2H 2 O by evaporation with a concentration degree > 6. In the following treatment, ~ 90% of residual Ca (0.6 g/l) can be selectively extracted with Na-D 2 EHPA. The subsequent solvent extraction step with Na-Cyanex 272 separates Co (> 99%) and Mg (> 95%). The resultant nickel sulfate solution (61.7 g/l Ni, 0.3 g/l Mg and Co 0.007 g/l) of > 99.5% purity can be directly integrated into state-of-the-art nickel recovery processes.

Keywords: extraction; purity; nickel recovery; industrial sidestream; high purity

Journal Title: JOM
Year Published: 2019

Link to full text (if available)


Share on Social Media:                               Sign Up to like & get
recommendations!

Related content

More Information              News              Social Media              Video              Recommended



                Click one of the above tabs to view related content.