Abstract Environmental barrier coatings (EBCs) are being developed to improve the durability of SiCf/SiC CMC components against harsh combustion environment. Among the most promising EBC candidates, rare-earth (RE) disilicates attract… Click to show full abstract

Abstract Environmental barrier coatings (EBCs) are being developed to improve the durability of SiCf/SiC CMC components against harsh combustion environment. Among the most promising EBC candidates, rare-earth (RE) disilicates attract attentions for the good thermal and chemical compatibility with SiC CMCs. We herein investigate the high temperature corrosion resistances of a new multicomponent β-(Er0.25Tm0.25Yb0.25Lu0.25)2Si2O7 disilicate subjected to hot water vapor and molten CMAS. Multicomponent (Er0.25Tm0.25Yb0.25Lu0.25)2Si2O7 shows superior water vapor corrosion resistance at 1400 °C and significantly enhanced CMAS resistance at 1500 °C compared with single principal RE disilicates. The present results highlight the merit of multiple RE engineering in advanced EBCs for the improvement of crucial high temperature corrosion resistances in engine applications.

Keywords: 25tm0 25yb0; temperature corrosion; high temperature; corrosion; er0 25tm0; 25yb0 25lu0

Journal Title: Corrosion Science
Year Published: 2020

Link to full text (if available)


Share on Social Media:                               Sign Up to like & get
recommendations!

Related content

More Information              News              Social Media              Video              Recommended



                Click one of the above tabs to view related content.