Electrical dual-percolation in MWCNTs/SBS/PVDF based thermoplastic elastomer (TPE) composites and the effect of mechanical stretching

Abstract Dielectric thermoplastic elastomers (TPEs) offer a number of advantages over traditional dielectric elastomers or rubbers in terms of tailorable mechanical and electrical properties, higher mechanical strain, and ease of… Click to show full abstract

Abstract Dielectric thermoplastic elastomers (TPEs) offer a number of advantages over traditional dielectric elastomers or rubbers in terms of tailorable mechanical and electrical properties, higher mechanical strain, and ease of processing and shaping. Such a combination of properties has attracted increasing attention in flexible energy harvesting and storage applications. The combination of styrene–butadiene-styrene (SBS) and poly(vinylidene fluoride) (PVDF) has the potential to provide a combination of high elongation to break and increased relative permittivity, however the immiscibility between SBS and PVDF results in polymer blends with poor stretchability and processing properties. In this work, a dual percolated structure was created in a thermoplastic elastomer of SBS/PVDF (50/50 wt%), by coupling EVA as a compatibiliser for SBS/PVDF with multi-walled carbon nanotubes (MWCNTs) as a conductive filler that created an electrical percolation network. The elongation at break of SBS/PVDF was significantly enhanced by adding 20 wt% of EVA due to the reduced phase dimensions and enhanced interfacial adhesion. The addition of MWCNTs enabled the formation of a percolated network at 1 wt% in the SBS phase, followed by a second percolation at 3 wt% in both PVDF and SBS phases. The relative permittivity of the composite increased to 22.5 at 1 wt% MWCNT with a tan δ of 0.5, and further increased to 34.9 for a 2 wt% of MWCNT concentration while the tan δ remained constant. In-situ electrical testing for the SBS/PVDF thermoplastic elastomer under strain showed that, at 1 wt% MWCNT, the non-percolated PVDF islands acted as variable capacitors whose capacitance increased with degree of stretching. For the dual percolated structure formed at 3 wt% MWCNT, the capacitance and conductivity of the composites were unaffected up to 30% strain. The high relative permittivity and strains of over 100% means that the SBS/PVDF based thermoplastic elastomer is readily suitable for vibration control sensors, variable impedance devices, energy harvesters and artificial muscles and actuators.

Keywords: sbs pvdf; percolation; thermoplastic elastomer

Journal Title: European Polymer Journal
Year Published: 2019

Link to full text (if available)


Share on Social Media:                               Sign Up to like & get
recommendations!

Related content

More Information              News              Social Media              Video              Recommended



                Click one of the above tabs to view related content.