Abstract In order to further improve the Nd3+:(LuxGd1-x)3Ga5O12 (Nd:LGGG) crystal performance in high power laser field, a long Nd:LGGG crystal with dimensions of Φ 23 × 112 mm3 has been grown successfully by… Click to show full abstract
Abstract In order to further improve the Nd3+:(LuxGd1-x)3Ga5O12 (Nd:LGGG) crystal performance in high power laser field, a long Nd:LGGG crystal with dimensions of Φ 23 × 112 mm3 has been grown successfully by the Czochralski (Cz) method for laser rod fabrication. Compared with the normal size LGGG crystals (like 30–50 mm in length), we overcame several difficulties in the growth of longer ones, including crystal cracking by a large longitudinal temperature gradient, spiral growth by a small radial temperature gradient, and growth instability and even constitutional super cooling by Ga2O3 volatilizing continuously. The doping concentrations of Nd3+ and Lu3+ in the as-grown crystal and the crystal optical quality have been measured. The performance of diode-side-pumped Nd:LGGG rod laser has been preliminarily tested for the first time, simply by replacing the Nd:YAG crystal rod inside a commercial laser module. Under an incident pump power of 160 W, the maximum continuous wave output power of 38 W has been obtained, corresponding to an optical-optical conversion efficiency of 23.8% and a slope efficiency of 40.8%, respectively.
               
Click one of the above tabs to view related content.