Abstract In this work, the Ti-6Al-4V alloy and ZrB2-SiC ultra-high temperature ceramic joint was brazed by TiCuZrNi amorphous filler at 910 °C with varied holding time. The element diffusion, microstructure and… Click to show full abstract
Abstract In this work, the Ti-6Al-4V alloy and ZrB2-SiC ultra-high temperature ceramic joint was brazed by TiCuZrNi amorphous filler at 910 °C with varied holding time. The element diffusion, microstructure and precipitation phase of the joints were analyzed in details. Reaction products in the joints were identified as β-Ti, (Ti,Zr)2(Cu,Ni), TiCu, Ti2Cu, TiC, Ti5Si3, TiB and TiB2. The formation schemes of reaction products were investigated. The holding time has substantial impacts on interfacial microstructure and shear strength of joints. A maximum shear strength of 345 MPa of the joint was reached under a brazing temperature of 910 °C and holding time of 1200 s. It is also found that the shear strength depends on the amount of eutectic structure and brittle compounds in the joints.
               
Click one of the above tabs to view related content.