A bimodal particle size distribution enhances mechanical and magnetocaloric properties of low-temperature hot pressed Sn-bonded La0.8Ce0.2(Fe0.95Co0.05)11.8Si1.2 bulk composites

Photo by maxwbender from unsplash

Abstract We report a Sn-bonded La0.8Ce0.2(Fe0.95Co0.05)11.8Si1.2 bulk composite with improved mechanical and magnetocaloric properties. La0.8Ce0.2(Fe0.95Co0.05)11.8Si1.2 powders with a bimodal particle size distribution were mixed with a binder of Sn powder… Click to show full abstract

Abstract We report a Sn-bonded La0.8Ce0.2(Fe0.95Co0.05)11.8Si1.2 bulk composite with improved mechanical and magnetocaloric properties. La0.8Ce0.2(Fe0.95Co0.05)11.8Si1.2 powders with a bimodal particle size distribution were mixed with a binder of Sn powder and hot pressed at a relatively low temperature of 423 K (150 °C). The use of bimodal size-distributed powder can reduce the non-magnetic Sn content. A bimodal particle size distribution of coarse particles (180–250 μm) and fine powders (

Keywords: fe0 95co0; la0 8ce0; bimodal particle; 95co0 8si1; 8ce0 fe0; size

Journal Title: Journal of Magnetism and Magnetic Materials
Year Published: 2019

Link to full text (if available)


Share on Social Media:                               Sign Up to like & get
recommendations!

Related content

More Information              News              Social Media              Video              Recommended



                Click one of the above tabs to view related content.