Microstructural characterization and comparison of Ti-6Al-4V manufactured with different additive manufacturing processes

Photo from wikipedia

Abstract In this work, the microstructures of Ti-6Al-4V manufactured by different additive manufacturing (AM) processes have been characterized and compared. The microstructural features that were characterized are the α lath… Click to show full abstract

Abstract In this work, the microstructures of Ti-6Al-4V manufactured by different additive manufacturing (AM) processes have been characterized and compared. The microstructural features that were characterized are the α lath thickness, grain boundary α (GB-α) thickness, prior β grain size and α colony size. In addition, the microhardnesses were also measured and compared. The microstructure of shaped metal deposited (SMD) Ti-6Al-4V material showed the smallest variations in α lath size, whereas the material manufactured with laser metal wire deposition-0 (LMwD-0) showed the largest variation. The prior β grain size was found to be smaller in material manufactured with powder bed fusion (PBF) as compared with corresponding material manufactured with the directed energy deposition (DED) processes. Parallel bands were only observed in materials manufactured with DED processes while being non-present in material manufactured with PBF processes.

Keywords: manufactured different; manufacturing processes; additive manufacturing; material; different additive; 6al manufactured

Journal Title: Materials Characterization
Year Published: 2018

Link to full text (if available)


Share on Social Media:                               Sign Up to like & get
recommendations!

Related content

More Information              News              Social Media              Video              Recommended



                Click one of the above tabs to view related content.