Abstract Chitosan with three different molecular weights (538 ± 48, 229 ± 45 and 13 ± 3 kDa) was used to develop biodegradable Inverted Colloidal Crystal (ICC) scaffolds with uniform pore size and interconnected pore network. Mass… Click to show full abstract

Abstract Chitosan with three different molecular weights (538 ± 48, 229 ± 45 and 13 ± 3 kDa) was used to develop biodegradable Inverted Colloidal Crystal (ICC) scaffolds with uniform pore size and interconnected pore network. Mass loss and compression modulus were analyzed after hydrolytic degradation in order to understand the influence of molecular weight on structural and mechanical degradation of chitosan ICC structures. Results show that medium molecular weight chitosan (229 ± 45 kDa) retains ICC structure and compression modulus for an extended period (4 weeks) and is therefore the preferred one for the production of ICC for soft tissue engineering.

Keywords: weight; weight structural; molecular weight; colloidal crystal; influence molecular; inverted colloidal

Journal Title: Materials Letters
Year Published: 2017

Link to full text (if available)


Share on Social Media:                               Sign Up to like & get
recommendations!

Related content

More Information              News              Social Media              Video              Recommended



                Click one of the above tabs to view related content.