Abstract l -Lactide was polymerized by means of neat SnOct2 with variation of LA/Cat ratio, temperature and time. The resulting cyclic polylactides crystallized spontaneously at 160 °C or below, but needed… Click to show full abstract
Abstract l -Lactide was polymerized by means of neat SnOct2 with variation of LA/Cat ratio, temperature and time. The resulting cyclic polylactides crystallized spontaneously at 160 °C or below, but needed nucleation via mechanical stress at 165 or 170 °C. All the crystalline polylactides obtained directly from ROP above 120 °C had melting temperatures (Tm) above 189 °C (up to 194.5 °C). SnOct2 also enabled transformation of low Tm poly( l -lactide)s (Tm
               