segregation behavior at grain boundaries for a three-phase ceramic Al2O3-MgAl2O4-8 mole% Y2O3 stabilized cubic ZrO2 (YSZ) made under different processing conditions: (1) conventional sintering, (2) flash sintering, and (3) spark… Click to show full abstract
segregation behavior at grain boundaries for a three-phase ceramic Al2O3-MgAl2O4-8 mole% Y2O3 stabilized cubic ZrO2 (YSZ) made under different processing conditions: (1) conventional sintering, (2) flash sintering, and (3) spark plasma sintering (SPS) [1,2] . Understanding the elemental segregation at grain boundaries and point defect generation in the bulk can provide practical knowledge of processing for desirable properties using grain boundary engineering.
               