The MnO2/LaMnO3 catalyst with the rod-like morphology designed by alkaline hydrothermal and acid etching treatment, performing 90% of toluene converted at 236 °C with a weight hourly space velocity... Click to show full abstract
The MnO2/LaMnO3 catalyst with the rod-like morphology designed by alkaline hydrothermal and acid etching treatment, performing 90% of toluene converted at 236 °C with a weight hourly space velocity...
               