Construction of an active composite as a biomarker with deeper tissue penetration and higher signal-to-noise ratio (SNR) is of great importance for the application in bioimaging. Here, we report a… Click to show full abstract
Construction of an active composite as a biomarker with deeper tissue penetration and higher signal-to-noise ratio (SNR) is of great importance for the application in bioimaging. Here, we report a strategy for tuning the emission bandwidth and intensity via crystal field control in long persistent phosphors (LPPs). Ni2+-doped Zn1+ySnyGa2−x−2yO4 phosphors, with a tunable emission band peaking from 1270 to 1430 nm in the second near-infrared (NIR) window, have been successfully prepared. Such featured materials have the advantages of low absorption and scattering as well as more efficient tissue penetration. The emission spectra can be controlled by tailoring the local crystal field around the activator precisely via substitution of Zn and Sn for Ga. Moreover, with high resolution and weak light disturbance, these developed multi-band afterglow phosphors exhibit great application potential in advanced optical imaging.
               
Click one of the above tabs to view related content.