ABSTRACT The (1-x)Na0.5Bi0.5TiO3- xBaTiO3 ceramics (x = 0.1, 0.135 and 0.17) were fabricated by a conventional solid phase sintering process. The bulk density of the obtained samples exceeded 95% of… Click to show full abstract
ABSTRACT The (1-x)Na0.5Bi0.5TiO3- xBaTiO3 ceramics (x = 0.1, 0.135 and 0.17) were fabricated by a conventional solid phase sintering process. The bulk density of the obtained samples exceeded 95% of the theoretical relative density as determined by Archimedes method. Dielectric and ferroelectric measurements of these ceramics were performed. Measurements of the ferroelectric properties show that, above the depolarization temperature Td, the shape of the hysteresis loops approaches that of linear dielectrics. The dielectric study results correlate with the hysteresis loops measurements. The relaxor-like behavior of the investigated materials was revealed.
               