Sr1−3x/2LaxTiO3 (SLTO) ceramics (x = 0.05, 0.10, 0.15) were prepared with giant dielectric constant by the traditional solid-state method at 1350∘C. The temperature dependence of the dielectric con... Click to show full abstract
Sr1−3x/2LaxTiO3 (SLTO) ceramics (x = 0.05, 0.10, 0.15) were prepared with giant dielectric constant by the traditional solid-state method at 1350∘C. The temperature dependence of the dielectric con...
               