Basalt fiber was first treated in a mixture of formic acid (FA) and dichloromethane (DCM) to reduce its diameter down to one micrometer. Electrospinning process was utilized to produce treated… Click to show full abstract
Basalt fiber was first treated in a mixture of formic acid (FA) and dichloromethane (DCM) to reduce its diameter down to one micrometer. Electrospinning process was utilized to produce treated basa...
               