LaNiO3 coated LiNi0.5Co0.2Mn0.3O2 (NCM523) materials were successfully synthesized via a sol-gel method. Morphological measurements indicate that LaNiO3 layer with ∼10 nm thickness was coated unifo... Click to show full abstract
LaNiO3 coated LiNi0.5Co0.2Mn0.3O2 (NCM523) materials were successfully synthesized via a sol-gel method. Morphological measurements indicate that LaNiO3 layer with ∼10 nm thickness was coated unifo...
               