Mechanical Properties of Bisacryl-, Composite-, and Ceramic-resin Restorative Materials.

Photo from wikipedia

OBJECTIVE Resin-based materials used in restorative dentistry are introduced at a fast pace with limited knowledge about their properties. Comparing properties of these materials from different restorative categories is lacking… Click to show full abstract

OBJECTIVE Resin-based materials used in restorative dentistry are introduced at a fast pace with limited knowledge about their properties. Comparing properties of these materials from different restorative categories is lacking but can help the clinician in material selection. This study aimed to compare mechanical properties and wear resistance of bis-acryl-, composite-, and ceramic-resin restorative materials. METHODS AND MATERIALS Bisacryl-resin (Bis-R, LuxaCrown, DMG), composite-resin (Com-R, Filtek Supreme Ultra, 3M Oral Care), and ceramic-resin (Cer-R, Enamic, VITA Zahnfabrik) specimens were prepared for mechanical tests: fracture toughness (FT) with and without initial thermomechanical loading using a mastication simulator, flexural strength (FS), and flexural modulus (FM), compressive strength (CS), and volumetric wear loss measurement. The datasets for FT and wear resistance were each analyzed using two-way ANOVA followed by pairwise comparisons or Tukey testing as appropriate. The datasets for FS, FM, and CS were analyzed using one-way ANOVA followed by the Tukey test. RESULTS Analysis of FS, FM, and CS showed significant differences between materials, with all pairwise comparisons between materials showing significance. Analysis of FT resulted in a significant interaction between the material and treatment, with analysis of wear loss showing a significant interaction between the material and the number of cycles. CONCLUSIONS Cer-R demonstrated superior FT, CS, and wear resistance compared to Bis-R and Comp-R materials. Fracture toughness of Bis-R increased after thermomechanical loading.

Keywords: restorative materials; mechanical properties; composite ceramic; ceramic resin; resin restorative; resin

Journal Title: Operative dentistry
Year Published: 2022

Link to full text (if available)


Share on Social Media:                               Sign Up to like & get
recommendations!

Related content

More Information              News              Social Media              Video              Recommended



                Click one of the above tabs to view related content.