Calibration of Electrical Resistance to Moisture Content for Beech Laminated Veneer Lumber “BauBuche S” and “BauBuche Q”

Photo by enchaxcreative from unsplash

Electrical resistance measurements are often employed for the purpose of nondestructive long-term monitoring of wood moisture content (MC) in timber structures. As a structural material for high-performance load-bearing applications in… Click to show full abstract

Electrical resistance measurements are often employed for the purpose of nondestructive long-term monitoring of wood moisture content (MC) in timber structures. As a structural material for high-performance load-bearing applications in such structures, beech laminated veneer lumber (LVL) enjoys a growing popularity. However, due to the processing of beech LVL affecting physical properties, calibration curves for bulk beech wood cannot be used. In this study, resistance was measured on 160 beech LVL samples equilibrated in four different relative humidity (RH) climates. The results show a difference not only between the beech LVL products “BauBuche S” and “BauBuche Q”, but also between measurements at two different depths. For each data set, parameters for calibration models using two and using three model parameters were determined by regression analysis to MC determined by the gravimetric method.

Keywords: electrical resistance; baubuche; beech laminated; resistance; moisture content

Journal Title: Forests
Year Published: 2021

Link to full text (if available)


Share on Social Media:                               Sign Up to like & get
recommendations!

Related content

More Information              News              Social Media              Video              Recommended



                Click one of the above tabs to view related content.