The paper describes the method for producing WC-10wt%Co hard alloy with 99.6% of the theoretical density and a Vickers hardness of ~1400 HV 0.5. Experimental data on densification dynamics, phase… Click to show full abstract
The paper describes the method for producing WC-10wt%Co hard alloy with 99.6% of the theoretical density and a Vickers hardness of ~1400 HV 0.5. Experimental data on densification dynamics, phase composition, morphology, mechanical properties, and grain size distribution of WC-10%wtCo using spark plasma sintering (SPS) within the range of 1000–1200 °C are presented. The high quality of the product is provided by the advanced method of high-speed powder mixture SPS-consolidation at achieving a high degree of densification with minimal calculated grain growth at 1200 °C.
               