Published in 2020 at "Journal of Materials Engineering and Performance"
DOI: 10.1007/s11665-020-04762-5
Abstract: The oxidation behavior of superalloys has attracted more attention due to the increasing service temperature of components in aero-engines. In this study, the isothermal oxidation behavior of a Ni-20Cr-18W superalloy has been investigated at 900…