Articles with "1mo alloy" as a keyword



Thermal expansion properties of laser melting deposited Ti-6.5Al-2Zr-1Mo-1V alloy during α + β zone annealing

Sign Up to like & get
recommendations!
Published in 2017 at "Materials Characterization"

DOI: 10.1016/j.matchar.2017.01.019

Abstract: Abstract Thermal expansion properties of laser melting deposited Ti-6.5Al-2Zr-1Mo-1V alloy during α + β zone annealing have been investigated based on dilatometry. The texture of deposited Ti-6.5Al-2Zr-1Mo-1V alloy was analyzed by electron back-scattered diffraction (EBSD) and the… read more here.

Keywords: 2zr 1mo; deposited 5al; expansion; 1mo alloy ... See more keywords
Photo by creativejunkie from unsplash

Investigation on microstructure and texture evolution of Ti–6Al–3Nb–2Zr–1Mo alloy during hot deformation

Sign Up to like & get
recommendations!
Published in 2021 at "Materials Research Express"

DOI: 10.1088/2053-1591/ac16ae

Abstract: Hot compression tests of Ti–6Al–3Nb–2Zr–1Mo alloy were conducted in the temperature range of 900 °C–1100 °C and strain rate range of 0.01–1s−1. Based on the true stress – true strain curve, the calculated activation energy… read more here.

Keywords: 2zr 1mo; 1mo alloy; texture; 3nb 2zr ... See more keywords

Hot working behaviour of Ti–8Al–1Mo–1V alloy through the hot compression test

Sign Up to like & get
recommendations!
Published in 2024 at "Materials Science and Technology"

DOI: 10.1177/02670836231223807

Abstract: Hot deformation behaviour of Ti–8Al–1Mo–1V alloy (Ti-811) was investigated through the hot compression tests at the temperatures of 950–1075 °C and at strain rates of 0.001–1 s−1. The flow curves of the Ti-811 alloy were successfully modelled… read more here.

Keywords: behaviour 8al; 8al 1mo; hot compression; alloy ... See more keywords

Effects of Cold Swaging on Mechanical Properties and Magnetic Susceptibility of the Zr–1Mo Alloy

Sign Up to like & get
recommendations!
Published in 2018 at "Metals"

DOI: 10.3390/met8060454

Abstract: Zr alloy is expected to decrease the artifact volume of magnetic resonance imaging (MRI) due to its relatively small magnetic susceptibility. To improve the mechanical properties of a Zr–1mass%Mo alloy that yielded a reduced artifact… read more here.

Keywords: alloy; 1mo alloy; cold swaging; mechanical properties ... See more keywords