Abstract: Abstract La0.67Ca0.33MnO3:Ag0.2 thin films were obtained by pulsed laser deposition followed by post-annealing at 1200 °C for varied durations. Surface morphologies, structures, and electrical and magnetic properties of films prepared with different annealing durations were significantly…