Published in 2018 at "Metals and Materials International"
DOI: 10.1007/s12540-018-00209-8
Abstract: To explore the ductility, a novel Mg–8.41Li–1.80Al–1.77Zn (designated as LAZ822) alloy was fabricated by casting, hot rolling and friction stir processing. The maximum elongation to failure of 489.5% was demonstrated in a fine-grained LAZ822 alloy…
read more here.