Published in 2021 at "Ceramics International"
DOI: 10.1016/j.ceramint.2021.01.131
Abstract: Abstract LCNMO (La0.7Ca0.26Na0.04MnO3) ceramics are prepared via the sol-gel method and sintered at different temperatures, ranging from 1000 to 1300 °C. The influences of sintering temperature on structure and electrical properties are systematically investigated. X-ray diffraction…
read more here.
Keywords:
la0 7ca0;
resistivity;
sintering temperature;
7ca0 26na0 ... See more keywords