The improvement of the self-healing ability of MoSi2 coatings at 900–1200 °C by introducing SiB6

Sign Up to like & get
recommendations!
Published in 2020 at "Journal of The European Ceramic Society"

DOI: 10.1016/j.jeurceramsoc.2020.01.048

Abstract: Abstract The brittleness of MoSi2 ceramic and the thermal mismatch between MoSi2 coating and C / C composite lead to brittle cracking of the coating at 900−1200 °C. This problem has been overcome in this studyby… read more here.

Keywords: mosi2 coatings; sib6; mosi2; 900 1200 ... See more keywords