Published in 2018 at "Integrated Ferroelectrics"
DOI: 10.1080/10584587.2018.1445372
Abstract: ABSTRACT In this study, the effects of calcination temperature (600–900°C for 2 h) and sintering temperature (1100–1200°C for 2 h) on phase formation, microstructure and electrical properties of new 0.94(Bi0.5Na0.5TiO3)-0.06(Ba0.945Ca0.055)(Ti0.91Sn0.09)O3 (0.94BNT-0.06BCTS) lead-free piezoelectric ceramics were…