Published in 2020 at "Ceramics International"
DOI: 10.1016/j.ceramint.2019.09.248
Abstract: Abstract B2O3 and Li2O (B/L)-added Ba0.6Sr0.4TiO3 (BST) ceramics sintered at 940 °C exhibited a dense microstructure with large grains. The amount of B/L additive was 4.5 wt% with a B/L ratio of 1.5:1. The B/L-related liquid phase…
read more here.