Published in 2017 at "Engineering Failure Analysis"
DOI: 10.1016/j.engfailanal.2017.08.027
Abstract: Abstract Failure of AISI 310 stainless steel tubes, used as radiant tubes in a heat treatment furnace, operating at temperature range 480 to 700 °C, is investigated. Longitudinal cracks were observed in tubes after around five…
read more here.
Keywords:
failure aisi;
sigma phase;
failure;
aisi 310 ... See more keywords
Sign Up to like & get
recommendations!
0
Published in 2019 at "Journal of hazardous materials"
DOI: 10.1016/j.jhazmat.2019.04.032
Abstract: Two stainless steel anodes, AISI 420 and AISI 310, and pure iron were compared in an electrocoagulation study for the simultaneous removal of phosphates, Orange II and Zinc ions from a synthetic wastewater at a…