Published in 2021 at "Materials"
DOI: 10.3390/ma14247490
Abstract: Magnetron-sputtered thin films of titanium and zirconium, with a thickness of 150 nm, were hydrogenated at atmospheric pressure and a temperature of 703 K, then anodized in boric, oxalic, and tartaric acid aqueous solutions, in…
read more here.