Published in 2017 at "Fusion Engineering and Design"
DOI: 10.1016/j.fusengdes.2017.03.070
Abstract: Abstract Alumina coating, with a thickness of 1 μm, has been manufactured by Pulsed Laser Deposition on EUROFER. A whole characterization of the interface, bare and coated, with stagnant Pb-17Li eutectic for 1000 h at 550 °C was…