Published in 2018 at "Ionics"
DOI: 10.1007/s11581-018-2633-0
Abstract: Conventional solid-state reaction method that is widely adopted to synthesize Li4Ti5O12 (LTO) typically generates rutile TiO2 phase at calcination temperature range between 700 and 900 °C in which two competitive reactions between anatase-to-rutile TiO2 and Li2TiO3-to-Li4Ti5O12…