Published in 2018 at "Journal of Materials Science: Materials in Electronics"
DOI: 10.1007/s10854-018-0030-0
Abstract: Pure K0.5Na0.5NbO3 lead-free piezoelectric ceramics without any dopants/additives were sintered at various temperatures (950–1125 °C) in low pO2 atmosphere (pO2 ~ 10−6 atm). All ceramics exhibit high relative densities (> 94%) and low weight loss (
read more here.
Keywords:
po2;
po2 atmosphere;
5na0 5nbo3;
ceramics sintered ... See more keywords
Sign Up to like & get
recommendations!
1
Published in 2017 at "Ceramics International"
DOI: 10.1016/j.ceramint.2017.01.058
Abstract: Abstract A polycrystalline SiC ceramic prepared by pressureless sintering of α-SiC powders with 3 vol% Al 2 O 3 -AlN-Y 2 O 3 additives in an argon atmosphere exhibited a high electrical resistivity of ~10 13…
read more here.
Keywords:
sic ceramics;
resistive sic;
microscopy;
highly resistive ... See more keywords
Sign Up to like & get
recommendations!
1
Published in 2017 at "Ceramics International"
DOI: 10.1016/j.ceramint.2017.05.246
Abstract: Abstract This study investigated the effects of sintering temperature and cooling rates on the positive temperature coefficient of resistance (PTCR) effect and microstructures of Ba 1.022 – x Sm x TiO 3 (BST) ceramics sintered…
read more here.
Keywords:
reducing atmosphere;
temperature;
effect microstructures;
ceramics sintered ... See more keywords
Sign Up to like & get
recommendations!
0
Published in 2018 at "Journal of Alloys and Compounds"
DOI: 10.1016/j.jallcom.2018.04.138
Abstract: Abstract Lead-free 0.4% MnO doped 0.955K0.5Na0.5NbO3-0.045Bi0.5Na0.5ZrO3 (Abbreviated as 0.955KNN-0.045BNZ) ceramics were prepared by a conventional solid-state sintering method in both ambient air and reducing atmosphere (H2/N2/H2O, oxygen partial pressure p o 2 = 1 × 10−10 atm). All samples…
read more here.
Keywords:
reducing atmosphere;
mno doped;
piezoelectric properties;
air ... See more keywords