Published in 2017 at "Integrated Ferroelectrics"
DOI: 10.1080/10584587.2017.1369309
Abstract: ABSTRACT Ni0.3Cu0.08Zn0.62Fe2O4 (NCZF) ceramics were prepared by solid state reaction route and calcined at temperatures at (i) 600°C for 30 minutes and (ii) 900°C for 15 minutes in microwave furnace. Room temperature X-ray diffraction analysis…