Tuning the Li/Ni Disorder of the NMC811 Cathode by Thermally Driven Competition between Lattice Ordering and Structure Decomposition

Sign Up to like & get
recommendations!
Published in 2020 at "Journal of Physical Chemistry C"

DOI: 10.1021/acs.jpcc.0c00720

Abstract: Ni-rich layered LiNixMnyCozO2 (NMC) cathodes for lithium-ion batteries are receiving a lot of attention owing to their promising large capacity, whereas the high content of Ni results in several is... read more here.

Keywords: thermally driven; tuning disorder; cathode thermally; disorder nmc811 ... See more keywords