Sign Up to like & get
recommendations!
1
Published in 2019 at "Ceramics International"
DOI: 10.1016/j.ceramint.2018.10.035
Abstract: Abstract In this paper, a 4 mol% MgO doped Zr0.92Y0.08O2-α (8YSZ) and its composite electrolyte of 8YSZ + 4MgO-NaCl/KCl were synthesized via a solid state reaction method. The morphology, structure and intermediate temperature electrochemical properties of the obtained…
read more here.
Keywords:
zr0 92y0;
doped zr0;
92y0 08o2;
electrolyte ... See more keywords
Sign Up to like & get
recommendations!
1
Published in 2019 at "Ceramics International"
DOI: 10.1016/j.ceramint.2018.11.148
Abstract: Abstract In this paper, 4 mol% ZnO-doped Zr0.92Y0.08O2-α (8YSZ) and its 8YSZ+4ZnO/NaCl-KCl composite electrolyte were synthesized by a solid-state reaction. The X–ray diffraction (XRD) analysis indicates that 8YSZ+4ZnO and inorganic chlorides phases can coexist. The inorganic…
read more here.
Keywords:
8ysz 4zno;
zr0 92y0;
mol zno;
doped zr0 ... See more keywords
Sign Up to like & get
recommendations!
1
Published in 2021 at "Ceramics International"
DOI: 10.1016/j.ceramint.2021.05.114
Abstract: Abstract High-quality ferroelectric films of Mn-doped Pb(Zr0.3Ti0.7)O3 (PMZT) were prepared using the sol-gel method, and the temperature dependence of ferroelectric, dielectric, and leakage current properties (J–E) were explored in detail using the top electrode/ferroelectric films/bottom…
read more here.
Keywords:
temperature dependence;
zr0 3ti0;
leakage;
doped zr0 ... See more keywords
Sign Up to like & get
recommendations!
0
Published in 2023 at "Phase Transitions"
DOI: 10.1080/01411594.2023.2205591
Abstract: ABSTRACT Ba(Zr0.02Ti0.98)O3 (BZT) samples with various weight percentages of Sm2O3 (0.02–0.06) were synthesized and calcined at 1100°C for 4 h. Circular pellets were prepared using calcined powders and sintered at 1450°C for 2 h. The sintered and…
read more here.
Keywords:
sm2o3;
zr0 02ti0;
study sm2o3;