Published in 2017 at "Journal of Applied Polymer Science"
DOI: 10.1002/app.44559
Abstract: The mechanical properties of ferromagnetic particle-reinforced silicone–rubber matrix composites are examined with quasi-static and dynamic nanoindentation measurements using Berkovich and flat punch indenters, respectively. Quasi-static nanoindentation is performed to examine primary factors such as the…