Low-cycle fatigue behavior of DZ125 superalloy under prior exposure conditions

Sign Up to like & get
recommendations!
Published in 2017 at "Rare Metals"

DOI: 10.1007/s12598-016-0874-5

Abstract: Low-cycle fatigue (LCF) behavior of the directionally solidified (DS) nickel-based DZ125 superalloy was studied at elevated temperature (980 °C). Specimens were, respectively, exposed for 0, 2, 25, 50, and 100 h in air. The fatigue life of… read more here.

Keywords: dz125 superalloy; cycle; cycle fatigue; low cycle ... See more keywords