Published in 2020 at "Scientific Reports"
DOI: 10.1038/s41598-020-69257-8
Abstract: A hierarchical microstructure strengthened high entropy superalloy (HESA) with superior cost specific yield strength from room temperature up to 1,023 K is presented. By phase transformation pathway through metastability, HESA possesses a hierarchical microstructure containing…