Sign Up to like & get
recommendations!
0
Published in 2020 at "Journal of Alloys and Compounds"
DOI: 10.1016/j.jallcom.2019.152935
Abstract: Abstract The recently developed Refractory Metal High Entropy Superalloys have the potential to replace Ni-based alloys in very high temperature structural applications. However, the microstructures of these new alloys typically consist of refractory metal based…
read more here.
Keywords:
refractory metal;
high entropy;
entropy superalloys;
refractory ... See more keywords
Sign Up to like & get
recommendations!
1
Published in 2020 at "Journal of Alloys and Compounds"
DOI: 10.1016/j.jallcom.2020.153983
Abstract: Abstract High-entropy superalloys (HESAs) can replace commercial Ni-based superalloys. For high-temperature applications, the oxidation resistance of HESAs must be considered. Herein, the oxidation mechanism of HESA with sufficient minor Nb addition was conducted at 900 °C…
read more here.
Keywords:
high entropy;
minor addition;
oxidation;
entropy superalloys ... See more keywords