Abstract: The Fe–Ni–P–Cu alloys with different copper content (0, 0.5, 1, and 2 wt%) are fabricated by liquid phase sintering (LPS) at 950 °C. The nano-Cu powder is mechanically mixed for 90 min with Fe–Ni–P composite powder using the…