Novel high Tg fully biobased poly(hexamethylene-co-isosorbide-2,5-furan dicarboxylate) copolyesters: Synergistic effect of isosorbide insertion on thermal performance enhancement

Sign Up to like & get
recommendations!
Published in 2019 at "Polymer Degradation and Stability"

DOI: 10.1016/j.polymdegradstab.2019.108983

Abstract: Abstract Here an effective solution for overcoming the low glass transition temperature (Tg) of poly(hexamethylene 2,5-furan dicarboxylate) (PHF), a fully biobased polyester derived from dimethylfuran-2,5-furan-dicarboxylate (DMFD) and 1,6-hexanediol (1,6-HD), is proposed that uses isosorbide (Is)… read more here.