Sign Up to like & get
recommendations!
1
Published in 2023 at "Materials"
DOI: 10.3390/ma16020803
Abstract: In this paper, the hot tensile deformation of a GH3230 superalloy double-sheet was conducted under deformation temperatures ranging from 1123~1273 K and strain rates ranging from 0.001~0.2 s−1. The flow behavior of the GH3230 superalloy…
read more here.
Keywords:
deformation;
gh3230 superalloy;
double sheet;
hot tensile ... See more keywords