Articles with "gh4169 superalloy" as a keyword



Numerical and experimental investigations on fretting fatigue properties of GH4169 superalloy at the elevated temperature

Sign Up to like & get
recommendations!
Published in 2021 at "International Journal of Fatigue"

DOI: 10.1016/j.ijfatigue.2021.106274

Abstract: Abstract Fretting fatigue is a detrimental phenomenon in aeronautic industry, where the appropriate methods for crack location prediction and total life prediction are vital. In the present paper, both experimental and numerical approaches were developed… read more here.

Keywords: model; gh4169 superalloy; prediction; fretting fatigue ... See more keywords

Preparation of ultrafine-grained GH4169 superalloy by high-pressure torsion and analysis of grain refinement mechanism

Sign Up to like & get
recommendations!
Published in 2019 at "Journal of Alloys and Compounds"

DOI: 10.1016/j.jallcom.2018.10.385

Abstract: Abstract A grain refinement process for a GH4169 superalloy sheet was proposed with the following parameters: solid solution (1050 °C × 0.5 h), cold rolling (50% reduction rate), δ phase precipitation treatment (890 °C × 10 h), high-pressure torsion (HPT) (3, 4, and… read more here.

Keywords: high pressure; pressure torsion; grain refinement; gh4169 superalloy ... See more keywords

Hot deformation behavior and constitutive model of GH4169 superalloy for linear friction welding process

Sign Up to like & get
recommendations!
Published in 2018 at "Journal of Manufacturing Processes"

DOI: 10.1016/j.jmapro.2018.03.017

Abstract: Abstract In order to realize a better description about the plastic flow behavior in linear friction welding process of GH4169 superalloy, especially at the friction interface where rather elevated temperature and severe deformation happened, it… read more here.

Keywords: friction welding; linear friction; model; strain ... See more keywords

Microstructural characterization and mechanical property of GH4169 superalloy joints obtained by linear friction welding

Sign Up to like & get
recommendations!
Published in 2019 at "Journal of Manufacturing Processes"

DOI: 10.1016/j.jmapro.2019.06.032

Abstract: Abstract The solid-solution strengthened GH4169 superalloy is joined successfully by linear friction welding (LFW) at various welding parameters in this study. Supported by numerical simulation, the microstructural characterization and mechanical property of the linear friction… read more here.

Keywords: linear friction; friction welding; characterization mechanical; friction ... See more keywords

An Optimized Strain-Compensated Arrhenius Constitutive Model of GH4169 Superalloy Based on Hot Compression

Sign Up to like & get
recommendations!
Published in 2024 at "Materials"

DOI: 10.3390/ma17143400

Abstract: A precise constitutive model is essential for capturing the deformation characteristics of the GH4169 superalloy in numerical simulations of thermal plastic forming processes. Hence, the aim of this study was to develop a precise modified… read more here.

Keywords: gh4169 superalloy; constitutive model; arrhenius constitutive; model ... See more keywords

Development and Characterization of ZnO Piezoelectric Thin Film Sensors on GH4169 Superalloy Steel Substrate by Magnetron Sputtering

Sign Up to like & get
recommendations!
Published in 2022 at "Micromachines"

DOI: 10.3390/mi13030390

Abstract: At present, piezoelectric sensors are primarily applied in health monitoring areas. They may fall off owing to the adhesive’s durability, and even damage the monitored equipment. In this paper, a piezoelectric film sensor (PFS) based… read more here.