Sign Up to like & get
recommendations!
1
Published in 2018 at "Ceramics International"
DOI: 10.1016/j.ceramint.2018.03.128
Abstract: Abstract The bonding temperature was lowered by placing intermediate layers that are reactive with a glass bonding frit. A dense reactive intermediate layer, ~ 6 µm in thickness, was anchored on STS304 by aerosol deposition (AD).…
read more here.
Keywords:
glass frit;
glass;
intermediate layer;
aerosol deposition ... See more keywords
Sign Up to like & get
recommendations!
2
Published in 2017 at "IFAC-PapersOnLine"
DOI: 10.1016/j.ifacol.2017.08.2061
Abstract: Abstract We work with the case study of an industrial glass bonding system for truck cabins that presents interesting aspects of timing to be investigated. Specifically, the coordination of the different equipments must start and…
read more here.
Keywords:
control;
industrial glass;
bonding system;