Evolution of solidification and microstructure in laser-clad IN625 superalloy powder on GTD-111 superalloy

Sign Up to like & get
recommendations!
Published in 2021 at "Surface and Coatings Technology"

DOI: 10.1016/j.surfcoat.2021.127010

Abstract: Abstract Nickel-based superalloys, especially GTD-111, are widely used in the aerospace industry. Due to the high amount of Cr, the IN625 superalloy can be a good option for the surface protection of GTD-111. In this… read more here.