Published in 2019 at "Journal of Materials Science: Materials in Electronics"
DOI: 10.1007/s10854-019-00933-w
Abstract: Dilithium Succinate (DLiS), a third order non-linear optical single crystal was grown efficaciously by adopting slow evaporation technique (SEST) at 303 K. DLiS crystal crystallizes into rhombohedral system with unit cell parameters a = 12.05 Å, b = 12.05 Å, c = 10.65 Å with V = 1339 Å3.…
read more here.
Keywords:
laser damage;
damage threshold;
single crystal;
threshold ldt ... See more keywords
Sign Up to like & get
recommendations!
0
Published in 2017 at "Journal of Applied Physics"
DOI: 10.1063/1.5004081
Abstract: Many high-field/attosecond and ultrafast electron diffraction/microscopy experiments on condensed matter require samples in the form of free-standing membranes with nanometer thickness. Here, we report the measurement of the laser-induced damage threshold of 11 different free-standing…
read more here.
Keywords:
free standing;
laser damage;
nanometer membranes;
standing nanometer ... See more keywords
Sign Up to like & get
recommendations!
1
Published in 2021 at "Optical Engineering"
DOI: 10.1117/1.oe.60.3.031001
Abstract: Abstract. The guest editors summarizes the contributions to Special Section on Laser Damage V.
read more here.
Keywords:
laser damage;
section guest;
special section;
Sign Up to like & get
recommendations!
1
Published in 2022 at "Optics letters"
DOI: 10.1364/ol.474961
Abstract: PETAL (Petawatt Aquitaine Laser) is an ultrahigh-power laser dedicated to academic research that delivers sub-picosecond pulses. One of the major issues of these facilities is the laser damage on optical components located at the final…
read more here.
Keywords:
damage growth;
laser damage;
polarization;
damage ... See more keywords
Sign Up to like & get
recommendations!
1
Published in 2022 at "Optics letters"
DOI: 10.1364/ol.481048
Abstract: Fused silica is prone to damage under ultraviolet laser irradiation. Because they are key components to achieve fusion on high energy laser facilities, final fused silica optics are analyzed after each laser shot. The quantification…
read more here.
Keywords:
damage size;
laser damage;
damage;
calibration ... See more keywords
Sign Up to like & get
recommendations!
1
Published in 2017 at "Applied Sciences"
DOI: 10.3390/app7080838
Abstract: Laser-induced damage on fused silica optics remains a major issue that limits the promotion of energy output of large laser systems. Subsurface impurity defects inevitably introduced in the practical polishing process incur strong thermal absorption…
read more here.
Keywords:
impurity defects;
laser damage;
damage resistance;
optics ... See more keywords